Mechanical Properties Metric English Comments
Charpy Impact 13.0 J
9.59 ft-lb
Typical (Longitudinal)
Industeel CLC 1.2316 Prehardened (300HB) and Corrosion Resistant Mold Steel
Description: CLC 1.2316 is a 16%Cr 1% Mo with improved corrosion resistance properties, thanks to the chromium/molybdenum additions. The high cleanliness/homogeneity of the steel makes it specially ..
Charpy Impact 13.0 J
9.59 ft-lb
103°C Temper Temperature
Latrobe Staminal™ Shock Resisting Die Steel
Staminal is an air or oil hardening die steel containing a large percentage of nickel combined with a proper balance of other alloying elements for deep hardening and extreme toughness. For tools, ..