Polymer Property : Charpy Impact = 83.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 83.0 J
61.2 ft-lb
V-Notch, Longitudinal
Latrobe Lescalloy® AF 1410 VIM-VAR ; 9 in High Strength Alloy Steel
LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a variety of critical,..
Charpy Impact 83.0 J
61.2 ft-lb
Notch status not reported
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725) Age Hardened Strip
Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Strip samples. Other property values are typical of INCONEL® alloy 725.D..