Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 111 J @Temperature 316 °C |
81.9 ft-lb @Temperature 601 °F |
V-notch |
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Charpy Impact | 111 J @Temperature 427 °C |
81.9 ft-lb @Temperature 801 °F |
V-notch |
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |