Polymer Property : Charpy Impact = 75.9 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 75.9 J
56.0 ft-lb
Material Condition - ST&A<sub>4</sub>
Crucible Compaction Metals P/M 625 Corrosion Resistant Alloy
P/M 625 (chemically, UNS N06625) is produced by the Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The Crucible powder con..