Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 74.6 J | 55.0 ft-lb | V-notch |
QuesTek® Innovations Ferrium® C61™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C61™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |