Mechanical Properties Metric English Comments
Charpy Impact 73.0 J
53.8 ft-lb
Haynes 230® alloy plate
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 10% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 10% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 10% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 20% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 20% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 20% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 30% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 30% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 30% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 40% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 40% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 40% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 73.0 J

@Temperature 427 °C
53.8 ft-lb

@Temperature 801 °F
V-notch
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, hot rolled and 1232°C solution annealed plate
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 50% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 50% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, 50% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Charpy Impact 73.0 J
53.8 ft-lb
solution annealed (unknown temp)
Haynes 230® alloy, cold rolled and 1232°C solution annealed sheet
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..