Polymer Property : Charpy Impact = 71.5 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 97.0 J

@Temperature 400 °C
71.5 ft-lb

@Temperature 752 °F
V-notch. Short transverse direction. 47 HRC
Assab Steels DIEVAR Hot Work Steel
DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i..