Mechanical Properties Metric English Comments
Charpy Impact 65.0 J
47.9 ft-lb
Latrobe LSSâ„¢ 17-4 Precipitation Hardening Stainless Steel (ASTM Type 360)
TLS 17-4 is a precipitation hardening, martensitic stainless steel that exhibits excellent resistance to atmospheric and chemical corrosion. TLS 17-4 exhibits an excellent combination of high stren..
Charpy Impact 65.0 J
47.9 ft-lb
Longitudinal; Notch status not reported
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round
Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D..