Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 88.0 J | 64.9 ft-lb | Transverse; Notch status not reported |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D.. |
|||
Charpy Impact | 88.0 - 134 J | 64.9 - 98.8 ft-lb | typical annealed |
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Charpy Impact | 88.0 - 134 J | 64.9 - 98.8 ft-lb | typical annealed |
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |