Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 8.13 J | 6.00 ft-lb | V-Notch; Air Cooled from 1010°C; 535°C Temper Temperature |
Latrobe LSSâ„¢ H13 Tool Steel (ASTM H13) TLS H13 tool steel is a versatile chromium-molybdenum hot work steel that is widely used in hot work and cold work tooling applications. The hot hardness (hot strength) of H13 resists thermal fatigu.. |
|||
Charpy Impact | 8.13 J | 6.00 ft-lb | V-Notch; 593°C Temper Temperature |
Latrobe Viscount 44® Prehardened Tool Steel (ASTM H13S) Viscount 44 is a free-machining, prehardened, H13-type hot work tool steel. It is produced using special melting, forging, and heat treating processes which provide the optimum in control
and reprod.. |
|||
Charpy Impact | >= 8.13 J | >= 6.00 ft-lb | |
Weartech International WT-32 Cobalt Hardfacing & Wear Resistant Alloy Applications: engine valves and seatsInformation provided by Weartech International |
|||
Charpy Impact | >= 8.13 J | >= 6.00 ft-lb | |
Weartech International WT-21 Cobalt Hardfacing & Wear Resistant Alloy Applications: hot trimming & forging dies, high pressure high temperature valves, hot shears, valve seats, pump impellers, ringsInformation provided by Weartech International |
|||
Charpy Impact | 8.13 - 9.49 J | 6.00 - 7.00 ft-lb | RT |
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |
|||
Charpy Impact | >= 8.13 J | >= 6.00 ft-lb | |
Weartech International WT-25 Cobalt Hardfacing & Wear Resistant Alloy Information provided by Weartech International |