Polymer Property : Charpy Impact = 58.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 58.0 J
42.8 ft-lb
aged 1000 hours at 650°C (1200°F)
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Charpy Impact 58.0 J
42.8 ft-lb
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..