Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 75.0 J @Temperature -269 °C |
>= 55.3 ft-lb @Temperature -452 °F |
|
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform .. |
|||
Charpy Impact | >= 75.0 J @Temperature -50.0 °C |
>= 55.3 ft-lb @Temperature -58.0 °F |
|
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24 Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me.. |
|||
Charpy Impact | 75.0 J | 55.3 ft-lb | V-Notch, Longitudinal |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 13.5 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Charpy Impact | 75.0 J | 55.3 ft-lb | V-notch |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150 (Heated 621°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Charpy Impact | >= 75.0 J @Temperature -50.0 °C |
>= 55.3 ft-lb @Temperature -58.0 °F |
|
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34 Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion.. |
|||
Charpy Impact | >= 75.0 J @Temperature -50.0 °C |
>= 55.3 ft-lb @Temperature -58.0 °F |
|
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom.. |