Mechanical Properties Metric English Comments
Charpy Impact 30.0 - 50.0 J

@Temperature -17.8 °C
22.1 - 36.9 ft-lb

@Temperature 0.000 °F
Latrobe CBS-50â„¢ NiL VIM-VAR High Performance Carburizing Bearing and Gear Steel
CBS-50 NiL VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. The chemistry is engineered such that when suitably carburized and heat treated the case ..