Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 8.00 J | 5.90 ft-lb | Hardening Temperature- 1200°C; Tempering Temperature- 525°C |
Crucible Steel CPM® Rex® 76®(HS), AISI M48 High Speed Steel Rex® 76®(HS) CPM Rex 76 is a super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It is heat treatable to HRC 68-70. Its high carbon, vanadium and cobalt contents provide abrasion resis.. |