Charpy Impact 5.00 J
3.69 ft-lb
Haynes 625 alloy, plate after 16000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Charpy Impact 5.00 J
3.69 ft-lb
Haynes 625 alloy, plate after 16000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Charpy Impact 5.00 J
3.69 ft-lb
Haynes 625 alloy, plate after 4000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Charpy Impact 5.00 J
3.69 ft-lb
V Notch, when tempered at 400°F
Carpenter R.D.S.® Alloy Tool Steel (Oil-Hard) (AISI L6)
R.D.S. tool steel is an oil hardening die steel which combines extreme toughness with very little size change when heat treated. It is available as a DeCarb-Free product. DCF bars have been cold fin..
Charpy Impact 5.00 J

@Temperature -73.0 °C
3.69 ft-lb

@Temperature -99.4 °F
V-notch
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Charpy Impact 5.00 J

@Temperature -184 °C
3.69 ft-lb

@Temperature -299 °F
V-notch
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F))
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..