Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 63.0 J | 46.5 ft-lb | Hardening Temperature- 1120°C; Tempering Temperature- 540°C |
Crucible Steel CPM® 9V® Tool Steel CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced.. |