Polymer Property : Charpy Impact = 42.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 42.0 J
31.0 ft-lb
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Charpy Impact 42.0 J
31.0 ft-lb
50% cold rolled
Haynes Hastelloy® G-30® alloy, 50% cold rolled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Charpy Impact 42.0 J
31.0 ft-lb
aged 8000 hours at 650°C (1200°F)
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..