Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 35.0 - 55.0 J | 25.8 - 40.6 ft-lb | Notched; as built |
EOS MS1 Maraging Steel for DMLS 3D Printing EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us.. |