Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 6.10 J | 4.50 ft-lb | Notched |
CMW® 1000 AMS-T-21014 AMS-7725 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Charpy Impact | 6.10 J | 4.50 ft-lb | Notched |
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Charpy Impact | 6.10 J | 4.50 ft-lb | V-Notch; Air Cooled from 996°C; 205°C Temper Temperature |
Latrobe LSS™ MGR™ Tool Steel (ASTM A8) TLS MGR tool steel is an air-hardening tool steel that is characterized by a combination of very good toughness, intermediate wear resistance, and excellent dimensional stability in heat treatment. .. |