Polymer Property : Charpy Impact = 4.28 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 5.80 J

@Temperature 22.8 °C
4.28 ft-lb

@Temperature 73.0 °F
ISO179
Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced
TECAPEEK® ST is a multipurpose semi-crystaline material from the polyaryletherketone family based on PEKEKK that features improved mechanical properties at higher temperatures. The benefits of TECA..