Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact >= 50.0 J

@Temperature >=-50.0 °C
>= 36.9 ft-lb

@Temperature >=-58.0 °F
Industeel SUPERELSO® 500 Quenched and Tempered High Strength Steel for Pressure Equipment
Description: Superelso® 500 (SE 500) is a 500MPa (72ksi) yield strength quenched and tempered steel adapted for pressure equipment. SE 500 is manufactured via the electric furnace with dephosphor..
Charpy Impact >= 50.0 J

@Temperature >=-60.0 °C
>= 36.9 ft-lb

@Temperature >=-76.0 °F
Industeel SUPERELSO® 500HR Quenched and Tempered High Strength Steel for Wet H2S Service
Description: Superelso® 500 HR (SE 500 HR, "Hydrogen Resistant") is a 500MPa (72ksi) yield strength quenched and tempered steel adapted for pressure equipment operating under sour service conditi..