Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 35.3 J | 26.0 ft-lb | V-Notch; Air Cooled from 1024°C; 260°C Temper Temperature |
Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications... |
|||
Charpy Impact | 35.3 J | 26.0 ft-lb | V-Notch; Air Cooled from 1010°C; 260°C Temper Temperature |
Latrobe LSSâ„¢ H13 Tool Steel (ASTM H13) TLS H13 tool steel is a versatile chromium-molybdenum hot work steel that is widely used in hot work and cold work tooling applications. The hot hardness (hot strength) of H13 resists thermal fatigu.. |