Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 339 J @Temperature -73.0 °C |
250 ft-lb @Temperature -99.4 °F |
Typical V-Notch |
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 0% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |