Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 32.5 J | 24.0 ft-lb | V-notch |
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st.. |
|||
Charpy Impact | 32.5 J | 24.0 ft-lb | V-Notch; Air Cooled from 1024°C; 640°C Temper Temperature |
Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications... |