Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 32.0 J | 23.6 ft-lb | tempering at 600°C (1110°F). Hardened at 960°C (1760°F). Quenched in air. Tempered twice. |
Assab Steels CALMAX Plastic Mold Material CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo.. |