Mechanical Properties Metric English Comments
Charpy Impact 31.0 J
22.9 ft-lb
after 8000 hours at 650°C
Haynes 188 alloy, plate at RT after 8000 hours at 650°C (1200°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..