Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 13.6 - 27.1 J | 10.0 - 20.0 ft-lb | V-Notch |
Materion ToughMet® T2 CX 90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |