Mechanical Properties Metric English Comments
Charpy Impact >= 358 J

@Thickness 19.1 mm
>= 264 ft-lb

@Thickness 0.752 in
Annealed
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Charpy Impact >= 358 J

@Treatment Temp. 427 °C,
Thickness 19.1 mm
>= 264 ft-lb

@Treatment Temp. 801 °F,
Thickness 0.752 in
Annealed, aged for 2000h
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Charpy Impact >= 358 J

@Treatment Temp. 482 °C,
Thickness 19.1 mm
>= 264 ft-lb

@Treatment Temp. 900 °F,
Thickness 0.752 in
Annealed, aged for 2000h
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Charpy Impact >= 358 J

@Treatment Temp. 538 °C,
Thickness 19.1 mm
>= 264 ft-lb

@Treatment Temp. 1000 °F,
Thickness 0.752 in
Annealed, aged for 2000h
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Charpy Impact >= 358 J

@Treatment Temp. 593 °C,
Thickness 19.1 mm
>= 264 ft-lb

@Treatment Temp. 1100 °F,
Thickness 0.752 in
Annealed, aged for 2000h
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Charpy Impact 358 J
264 ft-lb
annealed
Haynes HR-160® alloy, annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Charpy Impact 358 J
264 ft-lb
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..