Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 31.2 J | 23.0 ft-lb | V-Notch; Air Cooled from 1010°C; As Quenched |
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12) TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste.. |