Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 24.4 J | 18.0 ft-lb | V-notch |
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |