Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 16.3 J | 12.0 ft-lb | V-Notch; Air Cooled from 1010°C; 370°C Temper Temperature |
Latrobe LSSâ„¢ H14 Tool Steel (ASTM H14) TLS H14 tool steel is a 5%-chromium hot work steel to which tungsten has been added for improved high-temperature properties and heat resistance. It is a deep-hardening, airhardening
steel that exh.. |
|||
Charpy Impact | 16.3 J | 12.0 ft-lb | 48 Aging at 504°C |
Latrobe Nitralloy® N™ VAC-ARC Premium Nitriding Steel NITRALLOY N is an age hardenable nitriding steel. The age hardening capability of the alloy permits the core strength to be developed while the surface is being nitrided. VAC-ARC remelting is employ.. |
|||
Charpy Impact | 16.3 J | 12.0 ft-lb | 1190°C Hardening Temperature, 550°C Tempering Temperature; 67 Rockwell Hardness C |
Crucible Compaction Metals CPM® VIM CRU® 20® CPM® VIM CRU® 20® is a vacuum induction melted, cobalt-free super high speed steel manufactured by the Crucible Particle Metallurgy (CPM®) process. VIM CRU processing is designed to meet the cle.. |
|||
Charpy Impact | 16.3 J | 12.0 ft-lb | Transverse C-notch |
Crucible Steel CPM® S35VN™ Stainless Steel CPM S35VN is a martensitic stainless steel designed to offer improved toughness over CPM S30V. It is also easier to machine and polish than CPM S30V. Its chemistry has been rebalanced so that it for.. |
|||
Charpy Impact | 16.3 - 17.6 J | 12.0 - 13.0 ft-lb | 0.009" V-Notch in soft side; struck on hard side; Heat Treated |
ATI Allegheny Ludlum K12® Dual Hardness Steel This is a roll bonded, dual hardness armor plate consisting of a high hardness front side to break up or flatten incoming projectiles while the back side functions to capture the projectile.The comp.. |
|||
Charpy Impact | 16.3 J | 12.0 ft-lb | V-Notch; Air Cooled from 941°C; 649°C Temper Temperature |
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7) TLS S7 Shock-Resisting tool steel is an air or oil hardening tool steel that is characterized by very high impact toughness. The combination of strength and high toughness makes S7 tool steel a cand.. |
|||
Charpy Impact | 16.3 J | 12.0 ft-lb | V-Notch |
Materion moldMAX® LH High Hardness Beryllium Copper Alloy Description: moldMAX® and PROtherm® are Brush Wellman's copper beryllium alloys specifically designed for the plastic processing industry. These alloys provide a combination of thermal conduct.. |