Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 203 J @Temperature 23.0 °C |
150 ft-lb @Temperature 73.4 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |