Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 185 J | >= 136 ft-lb | |
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenchi.. |