Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 13.56 J | 10.00 ft-lb | |
Crucible Steel CPM® S30V® Stainless Steel CPM S30V is a martensitic stainless steel designed to offer the best combination of toughness, wear resistance and corrosion resistance. Its chemistry has been specially balanced to promote the form.. |