Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 17.6 J | 13.0 ft-lb | V-Notch; Air Cooled from 1010°C; 650°C Temper Temperature |
Latrobe LSSâ„¢ H14 Tool Steel (ASTM H14) TLS H14 tool steel is a 5%-chromium hot work steel to which tungsten has been added for improved high-temperature properties and heat resistance. It is a deep-hardening, airhardening
steel that exh.. |
|||
Charpy Impact | 17.6 J | 13.0 ft-lb | 1150°C Hardening Temperature, 550°C Tempering Temperature; 65.6 Rockwell Hardness C |
Crucible Compaction Metals CPM® VIM CRU® 20® CPM® VIM CRU® 20® is a vacuum induction melted, cobalt-free super high speed steel manufactured by the Crucible Particle Metallurgy (CPM®) process. VIM CRU processing is designed to meet the cle.. |