Polymer Property : Charpy Impact = 104 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 104 J

@Treatment Temp. 649 °C,
Thickness 19.1 mm
76.7 ft-lb

@Treatment Temp. 1200 °F,
Thickness 0.752 in
Annealed, aged for 2000h
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Charpy Impact 104 J

@Temperature 427 °C
76.7 ft-lb

@Temperature 801 °F
V Notch; plate
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..