Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 10.8 J | 8.00 ft-lb | V-Notch; Oil Quenched from 927°C; 200°C Temper Temperature |
Latrobe LSSâ„¢ S5 Shock-Resisting Tool Steel (ASTM S5) TLS S5 Shock-Resisting tool steel is a silicon-manganese tool steel which exhibits the highest impact toughness among all of the "S" type steels. The high toughness and the ability to be hardened to.. |
|||
Charpy Impact | 10.8 - 16.3 J | 8.00 - 12.0 ft-lb | Austenitizing temp 1725°F, Tempering temp 400-1000°F |
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel Chromium-molybdenum alloyed steelA versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and sh.. |
|||
Charpy Impact | 10.8 J | 8.00 ft-lb | V-Notch; Oil Quenched from 954°C; 149°C Temper Temperature |
Latrobe LSS™ S1 Shock-Resisting Tool Steel (ASTM S1) TLS S1 Shock-Resisting tool steel is a medium-carbon steel which combines moderate hardness with good impact toughness. It is a deep-hardening, oil-hardening steel designed for shock and impact load.. |