Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 630 MPa @# of Cycles 100000 |
91400 psi @# of Cycles 100000 |
alternating direct-stress (zero mean stress) |
TIMET TIMETAL® 685 (Ti-6Al-5Zr-0.5Mo-0.25Si) Titanium Alloy High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: Germany Aerospace: 3.7154. France: T-A6ZD. UK Aerospace Specifications BS TA. 43, 44.Features: TIMETAL 685 possesses .. |