Polymer Property : Fatigue Strength = 880 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength <= 880 MPa

@# of Cycles 2.00e+6
<= 128000 psi

@# of Cycles 2.00e+6
ArcelorMittal MartINsite® 1500 Cold Rolled Steel
Description: The family of MartINsite steels extends ArcelorMittal's range of Ultra High Strength Steels (UHSS). These steels allow the realization of lightweight structural elements by a forming me..
Fatigue Strength <= 880 MPa

@# of Cycles 1.00e+7
<= 128000 psi

@# of Cycles 1.00e+7
ArcelorMittal MartINsite® 1500 Cold Rolled Steel
Description: The family of MartINsite steels extends ArcelorMittal's range of Ultra High Strength Steels (UHSS). These steels allow the realization of lightweight structural elements by a forming me..