Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 470 MPa @# of Cycles 1.00e+7 |
68200 psi @# of Cycles 1.00e+7 |
rod, smooth, direct stress (UTS = 791 MPa) |
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); STA Cold Formable Medium-Strength AlloyFeatures: This binary, age hardening alloy combines the easy formability and weldability of commercially pure titanium with improved mechanical properties, particu.. |