Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 675 MPa @# of Cycles 1.00e+7 |
97900 psi @# of Cycles 1.00e+7 |
smooth |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®.. |
|||
Fatigue Strength | 675 MPa @# of Cycles 1.00e+7 |
97900 psi @# of Cycles 1.00e+7 |
smooth |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Beta Forged + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the Beta Forged + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4.. |