Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | <= 425 MPa @# of Cycles 100000 |
<= 61600 psi @# of Cycles 100000 |
|
ArcelorMittal HSLA 360 High strength low alloy steel for cold forming, Hot Rolled Available in the following: S355MCDescription: Steels in the HSLA (High Strength Low Alloy) range are hardened by a combination of precipitation and grain size refining, resulting in high strength w.. |