Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 60.0 MPa @# of Cycles 1.00e+7 , Temperature 140 °C |
8700 psi @# of Cycles 1.00e+7 , Temperature 284 °F |
R = 0.1, 8 Hz, dry |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |