Mechanical Properties Metric English Comments
Fatigue Strength 38.0 MPa

@# of Cycles 1.00e+7
5510 psi

@# of Cycles 1.00e+7
Flexural fatigue; ASTM D 671
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Fatigue Strength 38.0 MPa

@# of Cycles 1.00e+6
5510 psi

@# of Cycles 1.00e+6
tensile fatigue
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..