Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | >= 54.0 MPa @Temperature 80.0 - 120 °C |
>= 7830 psi @Temperature 176 - 248 °F |
Average value: 61.7 MPa Grade Count:1 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Fatigue Strength | >= 54.0 MPa @Time 0.000 - 374000 sec |
>= 7830 psi @Time 0.000 - 104 hour |
Average value: 61.7 MPa Grade Count:1 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |