Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 338 MPa @# of Cycles 500000 |
49000 psi @# of Cycles 500000 |
|
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |