Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Fatigue Strength = 490 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 490 MPa

@# of Cycles 1.00e+7
71100 psi

@# of Cycles 1.00e+7
Sheet; Reverse Bend (UTS = 772 MPa)
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); STA
Cold Formable Medium-Strength AlloyFeatures: This binary, age hardening alloy combines the easy formability and weldability of commercially pure titanium with improved mechanical properties, particu..
Fatigue Strength <= 490 MPa

@# of Cycles 2.00e+6
<= 71100 psi

@# of Cycles 2.00e+6
ArcelorMittal HSLA 460 High strength low alloy steel for cold forming, Hot Rolled
Available in the following: S460MCDescription: Steels in the HSLA (High Strength Low Alloy) range are hardened by a combination of precipitation and grain size refining, resulting in high strength w..
Fatigue Strength <= 490 MPa

@# of Cycles 1.00e+7
<= 71100 psi

@# of Cycles 1.00e+7
ArcelorMittal HSLA 460 High strength low alloy steel for cold forming, Hot Rolled
Available in the following: S460MCDescription: Steels in the HSLA (High Strength Low Alloy) range are hardened by a combination of precipitation and grain size refining, resulting in high strength w..
Fatigue Strength <= 490 MPa

@# of Cycles 2.00e+6
<= 71100 psi

@# of Cycles 2.00e+6
ArcelorMittal FB 590 Hot rolled ferrite-bainite steel
Available in the following: uncoated (HDT590F)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: ..
Fatigue Strength <= 490 MPa

@# of Cycles 1.00e+7
<= 71100 psi

@# of Cycles 1.00e+7
ArcelorMittal FB 590 Hot rolled ferrite-bainite steel
Available in the following: uncoated (HDT590F)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: ..