Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | <= 352 MPa @# of Cycles 1.00e+8 |
<= 51100 psi @# of Cycles 1.00e+8 |
after 2% elongation and heat treatment |
ArcelorMittal 260 BH Bake hardening steel, Cold rolled Available in the following: uncoated (HC260B), electroglavanized (HC260B+ZE) and Extragal®/Galvannealed (HC260BD+Z)Description: The composition and processing of these steels are designed to promot.. |