Polymer Property : Fatigue Strength = 34.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 34.0 MPa

@# of Cycles 1.00e+7 ,
Temperature 704 °C
4930 psi

@# of Cycles 1.00e+7 ,
Temperature 1300 °F
r=0.1
AK Steel 409 ULTRA FORM® Stainless Steel
AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and ..