Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | <= 320 MPa @# of Cycles 2.00e+6 |
<= 46400 psi @# of Cycles 2.00e+6 |
|
ArcelorMittal IF 260 High strength IF steel, Cold rolled Available in the following: uncoated (HC260Y), electroglavanized (HC260Y+ZE) and Extragal®/Galvannealed (HX260YD+Z/+ZF)Description: These steels were designed to provide an excellent combination of.. |
|||
Fatigue Strength | <= 320 MPa @# of Cycles 1.00e+7 |
<= 46400 psi @# of Cycles 1.00e+7 |
|
ArcelorMittal IF 260 High strength IF steel, Cold rolled Available in the following: uncoated (HC260Y), electroglavanized (HC260Y+ZE) and Extragal®/Galvannealed (HX260YD+Z/+ZF)Description: These steels were designed to provide an excellent combination of.. |
|||
Fatigue Strength | <= 320 MPa @# of Cycles 2.00e+6 |
<= 46400 psi @# of Cycles 2.00e+6 |
|
ArcelorMittal FB 450 Hot rolled ferrite-bainite steel Available in the following: uncoated (HDT450F) and Extragal® (HDT450F+Z)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It compr.. |
|||
Fatigue Strength | <= 320 MPa @# of Cycles 1.00e+7 |
<= 46400 psi @# of Cycles 1.00e+7 |
|
ArcelorMittal FB 450 Hot rolled ferrite-bainite steel Available in the following: uncoated (HDT450F) and Extragal® (HDT450F+Z)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It compr.. |
|||
Fatigue Strength | <= 320 MPa @# of Cycles 2.00e+6 |
<= 46400 psi @# of Cycles 2.00e+6 |
|
ArcelorMittal H 260 Solid solution steel, Cold rolled Available in the following: uncoated (HC260P) and electrogalvanized (HC260P+ZE) Description: Solid solution steels are designed to provide high strength while maintaining good drawability. These ste.. |
|||
Fatigue Strength | <= 320 MPa @# of Cycles 1.00e+7 |
<= 46400 psi @# of Cycles 1.00e+7 |
|
ArcelorMittal H 260 Solid solution steel, Cold rolled Available in the following: uncoated (HC260P) and electrogalvanized (HC260P+ZE) Description: Solid solution steels are designed to provide high strength while maintaining good drawability. These ste.. |